Curious how people have done this.
My finish process consists of applying transtint dye, letting dry followed by 6 coats of Tung oil then two layers of poly. A long process takes about a week since Tung oil needs to dry ~24 hrs between coats.
I am thinking it may be easier to finish all the exposed surfaces first and then assemble. Any suggestions
Debra
-
I would not risk getting the oil on the gluing surfaces.
-
I finished after the glue up.
-
Yes I agree, assemble then finish. I think it is easier.
-
We are in the midst of an edit of a new video covering this exact subject. Hope to have it up on a new youtube channel soon.
Short answer - glue it up first, then apply finishes.