Hi Karl,
I can't speak for dmannnn, but I used something like a total of 12 coats in two applications a couple weeks apart. The finish feels to me like a semi-gloss or eggshell and to me really feels like a mildly textured powdercoat job. I myself did not use anything over the final coats. I think you'll see that it is good and hard.
I've only used black so far, but have three brand new cans of the red, deep green, and gold to try -- hopefully tomorrow.
Somewhere in the general topics is a thread where I outlined my procedure -- basically just follow the instructions on the cans and things will work out fine. BTW, I used three light coats of the SEM primer, about 5 minutes apart andthen waited, I think, about 90 minutes before starting with the hammerite.
Good luck, but remember, with lots of light coats, it's really hard to mess this up. I'm blind and was able to do a great job without any help.
-- Jim
Jim Rebman -- recovering audiophile
Equitech balanced power; uRendu, USB processor -> Musette DAC -> 5670 tube buffer -> Finale Audio F138 FFX -> Cain and Cain Abbys near-field).
s.e.x. 2.1 under construction. Want list: Stereomour II
All ICs homemade (speaker and power next)