My finish process consists of applying transtint dye, letting dry followed by 6 coats of Tung oil then two layers of poly. A long process takes about a week since Tung oil needs to dry ~24 hrs between coats.
I am thinking it may be easier to finish all the exposed surfaces first and then assemble. Any suggestions